Beschreibung:
Protein wastes (feathers, goat hair) and cellulosic wastes (corn cob, coconut husks) were collected and washed with detergent solution, thoroughly rinsed and sun dried for 2 days before drying in an oven, and then ground. One-half of ground material was carbonized at a maximum temperature of 500°C after mixing with H2SO4. The carbonized parts were pulverized; both carbonized and uncarbonized sorbents were sieved into two particle sizes of 325 and 625 μm using mechanical sieve. Sorbents of a given particle size were packed into glass column.Then, textile wastewater that had its physicochemical parameters previously determined was eluted into each glass column and a contact time of 60 and 120 mins was allowed before analysis. Results showed 48.15–99.98 percentage reduction of , EC, Cl−, BOD, COD, DO, TSS, and TDS, 34.67–99.93 percentage reduction of , EC, Cl−, BOD, COD, DO, TSS, and TDS, 52.83–97.95 percentage reduction of Pb2+, Ni2+, Cr3+and Mn2+and 34.59–94.87 percentage reduction of Pb2+, Ni2+, Cr3+and Mn2+. Carbonization, small particle, size and longer contact time enhanced the sorption capabilities of the sorbents. These show that protein and cellulosic wastes can be used to detoxify wastewater.
Print ISSN:
1687-806X
Digitale ISSN:
1687-8078
Thema:
Chemie und Pharmazie
,
Werkstoffwissenschaften, Fertigungsverfahren, Fertigung
Permalink