    Publication Date: 2019-06-28
    Description: A program was performed to address the mechanical and environmental needs of Stirling engine heater head and regenerator housing components, while reducing the dependence on strategic materials. An alloy was developed which contained no strategic elemental additions per se. The base is iron with additions of manganese, molybdenum, carbon, silicon, niobium, and ferro-chromium. Such an alloy should be producible on a large scale at very low cost. The resulting alloy, designated as NASAUT 4G-Al, contained 15 Mn, 15 Cr, 2 Mo, 1.5 C, 1.0 Si, 1.0 Nb (in weight percent) with a balance of Fe. This alloy was optimized for chemistry, based upon tensile strength, creep-rupture strength, fracture behavior, and fatigue resistance up to 800 C. Alloys were also tested for environmental compatibility. The microstructure and mechanic properties (including hardness) were assessed in the as-cast condition and following several heat treatments, including one designed to simulate a required braze cycle. The alloy was fabricated and characterized in the form of both equiaxed and columnar-grained castings. The columnar grains were produced by directional solidification, and the properties were characterized in both the longitudinal and transverse orientations. The NASAUT 4G-Al alloy was found to be good in cyclic-oxidation resistance and excellent in both hydrogen and hot-corrosion resistance, especially in comparison to the baseline XF-818 alloy. The mechanical properties of yield strength, stress-rupture life, high-cycle-fatigue resistance, and low-cycle-fatigue resistance were good to excellent in comparison to the current alloy for this application, HS-31 (X-40), with precise results depending in a complex manner on grain orientation and temperature. If required, the ductility could be improved by lowering the carbon content.
    Keywords: METALLIC MATERIALS
    Type: NASA-CR-185174 , DOE/NASA/0282-1 , NAS 1.26:185174 , R89-917447-32
    Format: application/pdf
    Location Call Number Expected Availability
    BibTip Others were also interested in ...
  • 2
    Publication Date: 2019-07-12
    Description: In the course of studies on the iron-rich multicomponent system Fe-Mn-Cr-Mo-Nb-Al-Si-C, work was concentrated on pertinent quinary and six-component combinations namely Fe-Mn-Al-Si-C, Fe-Cr-Al-Si-C and Fe-Mn-Cr-Al-Si-C which had been elaborated at 65, 72, and 80 wt pct Fe. Manganese acts as a strong stabilizer for the cementite carbide. Chromium seems to stabilize the iron aluminide Fe2Al5 which forms in a considerable amount within an alloy of nominal composition Fe(65)Mn(15)Cr(12)Al(5)Si(2)C(1) (percent by weight). Although the Mn3AlC carbide is, like Fe3AlC, a perovskite carbide, manganese does not appear to favor the formation of the perovskite carbide. Because of the relatively low sintering temperature (700 C), for al large portion of the samples equilibria conditions are not always reached.
    Keywords: METALLIC MATERIALS
    Type: Journal of Materials Science (ISSN 0022-2461); 23; 3113-311
    Format: text
    Location Call Number Expected Availability
    BibTip Others were also interested in ...
  • 3
    Publication Date: 2019-07-13
    Description: The oxidation and sulfidation of several novel iron-base superalloys were evaluated in high-temperature cyclic tests. The experimental austenitic alloys examined were modifications of NASAUT-4GA which were developed for Stirling-engine application. The weight gains and resulting surface scales were measured and analyzed. Mixed oxide scales were found to form on all specimens exposed above 871 C. The build-up of these scales led to a depletion of Mn and Cr in a zone adjacent to the oxides. In addition, the initial oxidation of the Fe-rich alloy was inhibited by a thin but tenacious Si layer which formed at the interface between oxides and the parent layer. Sulfidation tests using Na2SO4 coatings resulted in the formation of a protective spinel and alpha-Fe2O3 phases. Preferential attack of the carbide phase by hydrogen was not observed after 350 h at 871 C.
    Keywords: METALLIC MATERIALS
    Type: Alternate alloying for environmental resistance; Mar 02, 1986 - Mar 06, 1986; New Orleans, LA; United States
    Format: text
    Location Call Number Expected Availability
    BibTip Others were also interested in ...