ISSN:
1573-9139
Source:
Springer Online Journal Archives 1860-2000
Topics:
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
Notes:
Conclusions Scale growth in the channel of the metering component during the pouring of steel deoxidized by 2.2–2.5 kg/ton of aluminum is influenced by: the amount and composition of the nonmetal impurities; the material and construction of the component; and the method of supplying the metal to the ingot mold. Stable steel pouring is secured by using a fireclay (36% Al2O3) metering component with widened channel (depth 55 mm), and with full protection against secondary oxidation for the metal stream.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1007/BF01291365
Permalink