Publication Date:
2019-06-28
Description:
Mylar strips, 2.5 microns thick, uncoated and coated with 50A, 100A and 200A of Al, Pd, and Au/Pd were exposed on STS-5 in order to measure the erosion of mylar and to test means of protecting thin plastic foils commonly used for space experiments in low earth orbit. Analysis by optical microscopy, SEM and STEM investigation, EDX measurements, FTIR spectroscopy and weight loss measurements showed that while up to 75 percent of the uncoated mylar was eroded during exposure, thin coatings of the above metals can protect mylar for integrated oxygen-fluxes of at least 10 to the 21st atoms/sq cm.
Keywords:
CHEMISTRY AND MATERIALS (GENERAL)
Type:
AIAA PAPER 83-2636
Format:
text
Permalink