Conclusions 1. We constructed recrystallization diagrams for alloy TSM-4. The initial recrystallization temperature is 1250–1600°, depending on the degree of deformation. The recrystallization process is completed at 1700–1800° at all degrees of deformation investigated. 2. Finely dispersed carbide phases delay secondary recrystallization until solution of excess phases (∼2000°). 3. The plasticity is highest and the anisotropy of the properties along and across the rolling direction is lowest for plates of alloy TSM-4 annealed at 1300° for 1 h.