Abstract Stress-strain curves of slowly cooled and quenched Al-2·5 wt. % Cu alloy were studied in the temperature range 693 K to 773 K. The linear work-hardening coefficient, the fracture time, the yield stress and the fracture stress of annealed and quenched samples decreased with increasing deformation temperature and exhibited a minimum at 733 K. The X-ray analysis of the slowly cooled and quenched samples showed that the lattice parametera of Al-matrix and the ratioc/a of the tetragonal Θ-phase reached a minimum and a maximum value, respectively, at the dissolution temperature.