The Effects of Leaching Process to the TiO2 Synthesis from Bangka Ilmenite

, , , , , , and

Published under licence by IOP Publishing Ltd
, , Citation S Wahyuningsih et al 2018 IOP Conf. Ser.: Mater. Sci. Eng. 333 012049 DOI 10.1088/1757-899X/333/1/012049

1757-899X/333/1/012049

Abstract

Ilmenite mineral is a naturally occurring iron titanate (FeTiO3) and is abundant in nature. The separation of components into TiO2 and Fe2O3 must be expand. The purpose of this research is to synthesis TiO2 nanoparticles from the filtrate of Bangka ilmenite leaching process. Leaching of ilmenite was done with H2SO4 and HCl at various concentrations. The formation of TiO2 crystal determined by hydrolysis conditions and condensation reaction. TiO2 synthesized from the filtrate of sulfuric acid leaching that produced from TiO2 anatase phase when hydrolyzed in an aquaregia solvent and low concentrations of HCl (0.1M). Hydrolysis conditions at higher concentrations of HCl (1M) was produced TiO2 anatase-rutile phase. The synthesis of TiO2 from the filtrate of hydrochloric acid leaching was produced anatase phase. While the condition under the alcoholic solvent (2-propanol: H2O (v/v) = 9: 1) anatase phase crystallites grow in the temperature range up to 550 °C, above this temperature, TiO2 transform into rutile phase.

Export citation and abstract BibTeX RIS

Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.

Please wait… references are loading.