    Rheologica acta 37 (1998), S. 573-582 
    ISSN: 1435-1528
    Keywords: Key words Sharkskin melt ; fracture ; visual observation ; polybutadiene extrusion ; exit stretching ; qualitative modeling
    Source: Springer Online Journal Archives 1860-2000
    Topics: Chemistry and Pharmacology , Physics
    Notes: Abstract We studied the sharkskin melt fracture phenomena of polybutadiene (PBD), which exhibits similar flow properties and instabilities to linear low density polyethylene (LLDPE). The advantages of using PBD are that it exhibits larger distortions and slower development due to its high viscosity. By using a video camera with close-up lenses focused at the die exit, we observed the development of sharkskin in profile. It was shown that the sharkskin melt fracture develops with the cohesive failure at the die exit due to a peeling of surface layers as described by Howell and Benbow (1962). Oddly enough, this mechanism is similar to that proposed by Ovaici et al. (1998) for the extrusion of chocolate. A soap solution coating around the die exit to induce a slippery interface eliminated the sharkskin fracture, similar in the effect of fluoro-elastomer coating with LLDPE. Based on our visual observations, we qualitatively modeled the sharkskin fracture by modifying Cogswell‘s (1977) idea on exit stretching at the die exit and the force balance of Ovaici et al. on the ring formation of the chocolate extrusion.
    Type of Medium: Electronic Resource
    Location Call Number Expected Availability
    BibTip Others were also interested in ...
Close ⊗
This website uses cookies and the analysis tool Matomo. More information can be found here...