ISSN:
0933-5137
Keywords:
Chemistry
;
Polymer and Materials Science
Source:
Wiley InterScience Backfile Collection 1832-2000
Topics:
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
Description / Table of Contents:
Cavitation Erosion Tests with Polyamid-Specimens and Stainless-Steel-SpecimensThe Darmstadt vibratory cavitation erosion method, cavitation tests were performed on two materials: a proven chromium-nickel alloy and a recently introduced polyamid grade.Time studies based on the above test method resulted in pronounced damage to the chromium-nickel alloy, as documented in mass loss curves and specimen surface pictures.In contrast, all polyamid specimens sustained no damage, i.e. no mass loss, no surface damage resulted.
Notes:
Eim im Pumpenbau bewährter Chrom-Nickel-Stahlguß und eine neuartige Polyamidvariante wurden bei Kavitationserosionsbelastung im Magnetostriktionschwinger untersucht. Aufgrund der ermittelten Massenabtrags-Laufdauerkurven und Probenoberflächenbilder sind beim Stahlguß ausgeprägte Werkstoffschäden feststellbar. An allen Polyamidproben sind dagegen weder Massenverluste noch Beschädigungen der Probenoberflächen zu erkennen.
Additional Material:
10 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/mawe.19860171007
Permalink