ISSN:
1013-9826
Source:
Scientific.Net: Materials Science & Technology / Trans Tech Publications Archiv 1984-2008
Topics:
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
Notes:
With fly ash, metakaolin, slag and alkaline activator as raw materials, the geopolymericceramic was synthesized and the properties, such as the weight loss, compressive strength and thestructures, at high temperatures of 400~1200°C were measured. The weight loss is in the range of 8~13%from 400°C to 800°C. Comparing with the strength at room temperature, the compressive strength ofsamples is mostly increased at 400°C and all of them increased at 800°C. 9.65~28.32% strength declinesat 1200°C. The variation of the compressive strength with temperature is explained based on the analysesof the phases constitutes and the thermal properties of samples
Type of Medium:
Electronic Resource
URL:
http://www.tib-hannover.de/fulltexts/2011/0528/01/56/transtech_doi~10.4028%252Fwww.scientific.net%252FKEM.368-372.1529.pdf
Permalink