ISSN:
1662-9752
Source:
Scientific.Net: Materials Science & Technology / Trans Tech Publications Archiv 1984-2008
Topics:
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
Notes:
The effects of following four factors, which are laser power, assist gas pressure, cooling rate and scanning speed on the quality characteristics of laser cut 316L stainless steel tubes have been studied. 24 full factorial design and central composite design were used to evaluate optimum condition of process parameters. Regression analysis was used to develop empirical models for the combined effects of the independent process parameters on laser cut quality. As the results, it wasobserved that laser power, assist gas pressure and scanning speeds did the major effects on kerf width. The smallest kerf width was obtained with the condition of low laser power, assist gas pressure, scanning speed and moderate cooling rate. Calculated regression model was kerf width = 64.47 + 0.91W + 1.25P + 0.41S + 0.41C2 - 0.45P2
Type of Medium:
Electronic Resource
URL:
http://www.tib-hannover.de/fulltexts/2011/0528/02/09/transtech_doi~10.4028%252Fwww.scientific.net%252FMSF.475-479.277.pdf
Permalink