ISSN:
0021-8995
Keywords:
Chemistry
;
Polymer and Materials Science
Source:
Wiley InterScience Backfile Collection 1832-2000
Topics:
Chemistry and Pharmacology
,
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
,
Physics
Notes:
A series of polyurethane elastomers were studied in which the soft segment composition was a molecular weight advanced poly(ethylene ether carbonate)diol (2025 mol wt) and the hard segment composition was based on MDI/1,4-butanediol. These polyurethane elastomers had a constant soft segment composition and block length, a constant hard segment composition, but a variable hard segment block length and concentration (31.9-65.2 wt % hard segment). Properties such as rubbery plateau modulus, solvent resistance, melting point, hardness, tensile strength, and hard segment run length all improve with increasing hard segment concentration. DMA and DSC data indicate a partially phase mixed morphology. However, phase mixing must occur at domain boundaries since the soft segment Tg is nearly invariant with hard segment concentration. Annealing studies indicate that the optimum post-cure temperature, for 1 h, is about 175°C.
Additional Material:
11 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/app.1990.070410305
Permalink