Low-fusing dental porcelain was fused on titanium surface. The adhesion between the titaniumand porcelain was evaluated by three-point flexure test. It was shown that the failure of the titaniumporcelainpredominantly occurred at the alloy-oxide interface. Rutile phase was present on the interfacedebonding from porcelain. The influence of corrosion on bonding strength was also investigated. Theresults suggested that, after being immersed in artificial saliva with pH of 2.7, 5.4 and 7.0, no decreasingof the bonding strength of Ti-porcelain occurred