Poly([4-(methacryloyloxy) butyl]pentamethyldisiloxane), PMBPD, has been prepared for the first time. At the weight average molecular weight of 55,900, it is a clear, viscous liquid with a glass transition temperature, Tg, of 236K. Copolymers with methylmethacrylate have also been prepared. The homo-and copolymers, all of which have methacrylate backbones with pendant siloxane groups, were blended with poly(methyl-methacrylate), PMMA. Using the existence of a single Tg as a definition of miscibility, it was found that blends of either PMMA or PMBPD with random copolymers are miscible. However, in spite of a clear appearance, the blend of the two horriopolymers were found to have two distinct Tgs.
Additional Material:
1 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/pen.760221712
Permalink