ISSN:
0032-3888
Keywords:
Chemistry
;
Chemical Engineering
Source:
Wiley InterScience Backfile Collection 1832-2000
Topics:
Chemistry and Pharmacology
,
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
,
Physics
Notes:
Polyalkylenebenzoxazoles of high molecular weight (inherent viscosity values from 0.76 to 2.95) were prepared from 4,6-diaminoresorcinol dihydrochloride and aliphatic diacids in polyphosphoric acid by heating at 180 to 200°C for 3-5 h. Melting points of the polymers ranged from 148 to 423°C, depending on the length of the alkylene chain. Glass transition temperatures were relatively low, ranging from 50 to 100°C and did not show the pronounced odd/even effect noted for melting points. In all cases, rapid weight loss occurred above 400°C. No evidence for the formation of a molecular composite was observed in an attempt to prepare in situ a rod-like polybenzoxazole in a polyalkylenebenzoxazole.
Additional Material:
2 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/pen.760340411