Hydrostatic extrusion of high density polyethylene at an extrusion ratio of 15:1 was investigated in the temperature range between 100 and 134°C. A thin-walled tube was extruded having a tensile strength of 370 MPa and a tensile modulus of 10 GPa. The extrusion rate was limited by severe extrudate distortion which occurs at a limiting shear stress under stick-slip conditions. Even during steady extrusion wall slip was evident. At a constant extrusion speed, the extrusion pressure was found to be very sensitive to the extrusion temperature. An increase from 120 to 125°C reduced the extrusion pressure by half. Various thermal pretreatments of the starting billets were found to have little effect on the extrusion behavior and physical properties of the extrudate.
Additional Material:
15 Ill.
Type of Medium:
Electronic Resource
URL:
http://dx.doi.org/10.1002/pen.760181115
Permalink