Abstract Low-cyclic fatigue test results are presented for samples cut in the axial and tangential direction from bimetallic tubing (base metal-steel 10GN2MFA + steel cladding 05Kh19N10G2B). The steel cladding material tends to contain multiple hot cracks of sizes up to 2 mm in the radial, and up to 5 mm in the axial direction. It was shown that a cyclic load Rσ≈O at maximum stress levels σmax = 350–400 MPa either did not lead to a change in the initial tears, or caused an increase in their size which did not exceed 0.3–0.7 mm.