Ceramic oxidation coating of approximately 60 [removed info]m thick was prepared on a Ly12 alloysubstrate by micro-plasma oxidation in an alkali-silicate electrolytic solution. Coating thickness wasmeasured during coating formation. The influence of current density, electrolyte temperature andinter-electrode distance on coating kinetics was investigated. Microstructure and phase compositionswere analyzed. The micro-hardness of the coating was also measured. The tribological performance of thecoatings was evaluated using a dry sand abrasion test. In addition, the results are compared to detonationsprayedalumina coating
Type of Medium:
Electronic Resource
URL:
http://www.tib-hannover.de/fulltexts/2011/0528/01/56/transtech_doi~10.4028%252Fwww.scientific.net%252FKEM.368-372.1271.pdf
Permalink