Description:
We investigated the influence of CuO amount (0.5–3.0 mol%), sintering temperature (900°C–1000°C), and sintering time (2–6 h) on the low-temperature sintering behavior of CuO-added Bi 0.5 (Na 0.78 K 0.22 ) 0.5 TiO 3 (BNKT22) ceramics. Normalized strain ( S max / E max ), piezoelectric coefficient ( d 33 ), and remanent polarization ( P r ) of 1.0 mol% CuO-added BNKT22 ceramics sintered at 950°C for 4 h was 280 pm/V, 180 pC/N, and 28 μC/cm 2 , respectively. These values are similar to those of pure BNKT22 ceramics sintered at 1150°C. In addition, we investigated the performance of multilayer ceramic actuators made from CuO-added BNKT22 in acoustic sound speaker devices. A prototype sound speaker device showed similar output sound pressure levels as a Pb(Zr,Ti)O 3 -based device in the frequency range 0.66–20 kHz. This result highlights the feasibility of using low-cost multilayer ceramic devices made of lead-free BNKT-based piezoelectric materials in sound speaker devices.
Print ISSN:
0002-7820
Electronic ISSN:
1551-2916
Topics:
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
Permalink