Depolarization ratios ρ of the Raman bands due to CH3 stretching at 2907 cm-1 and the Si—O skeletal mode at 491 cm-1 have been measured in polydimethylsiloxane gum as a function of temperature from 100°C to -45°C. Below 0°C the changes in p have been interpreted in terms of the formation of helical regions in the gum. The enthalpy of helix formation ΔH has been determined as 3200 ± 600 cal/mole. An upper limit on the entropy change, ΔS, of 16 ± 3 e.u./mole and minimum values of helix content at different temperatures have been found. The Raman spectrum of crystalline polydimethylsiloxane is presented.