The solvent debinding processes of wax-based binders in powder injection moldedTi(C,N)-based cermets were studied. Effects of debinding temperature, debinding time, samplethickness, solvent types and solvent concentration on binder removal were investigated. Also, thedimension change of samples during the solvent debinding process was studied. It can be found thatupwards of 70% paraffin waxes were removed and open pore channels were formed basically whenthe samples were immersed in heptane for 6 h at 50 °C